Pessy Posted October 3, 2021 Report Share Posted October 3, 2021 I had a fully loaded kiln, where I might've used wax resist excessively, and possible started firing before the wax was dry. My smoke alarm went off at 700 degrees, so I stopped the kiln, and unloaded. The wax on all the pieces are burnt, and the shelves appear slightly burnt too. Is this normal? I've never before checked what happens during the firing process. If this is ok, can I reload and fire again? Will the results be affected by my stopping the kiln? Quote Link to comment Share on other sites More sharing options...
Hulk Posted October 3, 2021 Report Share Posted October 3, 2021 (edited) Hi Pessy! I use wax on almost every piece - to get a sharp boundary/transition at the rim between liner glaze and outside/color glaze - hence a strong odor early in the firing cycle, but not enough to make clouds of smoke. No doubt the wax (along with glaze ingredients that burn away) is designed to fully burn away; I've not noticed any marking where the wax was, any road. Hence, my guess would be normal on question one. As for re-firing, I haven't (yet) had the experience of re-starting an interrupted glaze cycle, however, reading indicates yes on question two and no on three. I'm curious to know if the wax burns more cleanly with an air supply? I've fitted my (also somewhat ancient) Skutt with a kiln vent, which pulls a small stream of air from the bottom of the kiln, hence, small streams of air are pulled in through the various cracks, as well as the small holes drilled in the lid. Kiln venting is recommended for longer element life, more thorough bisque burnout, and nicer glaze colours. While the kiln vent helps quite a bit with the fumes, I did not feel comfortable being in the studio, at all, during firing, so have also set up an overhead rig to pull heat and fumes; it's noisy, but works well. Edited October 3, 2021 by Hulk normal Bill Kielb 1 Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted October 3, 2021 Report Share Posted October 3, 2021 (edited) 7 hours ago, Pessy said: If this is ok, can I reload and fire again? Will the results be affected by my stopping the kiln? Yes it is ought to be just fine. Wax burns off at around 800 degree f so in the range of let’s say 450 degrees to maybe 850 degrees folks often smell the wax. Use a lot of wax, lots of smell. You should not see any signs of carbon as it will burn away in the rest of the firing. Any kiln vent will help this but downdraft vents are often not capable of removing the smell completely …… and they are not really designed to get all the wax smell. So a downdraft will help but not likely to capture all of the wax smell. The smell will however disappear above 800 degrees. As far as refiring, a simple general way to think of this would be: for a glaze firing, if you have not fired within 300-400 degrees of you finish temperature then you have not done much real heatwork. Silica and alumina don’t melt less than 3000 degrees so they need flux and enough kiln energy to help them melt earlier. Until your kiln reaches this melting temperature (often called a eutectic) not much is done in the way of useful work on the glaze. So refiring is generally just fine for most. Technically (Per the Orton cone chart) most of the relevant heatwork to maturity is done in the last 200 - 250 degrees of the firing. For bisque firing, generally it’s not a concern, just rebisque to your proper cone. Generally It’s ok to bisque more than once and often done when multiple layers of decoration are desired. Edited October 3, 2021 by Bill Kielb Hulk and Gusf 2 Quote Link to comment Share on other sites More sharing options...
Pessy Posted October 3, 2021 Author Report Share Posted October 3, 2021 Thanks to both of you. I restarted the kiln an hour ago. I will keep you posted with the results Bill Kielb 1 Quote Link to comment Share on other sites More sharing options...
SUZANNEHIG Posted April 23, 2023 Report Share Posted April 23, 2023 How did things turn out? I just had the same issue. I turned the kiln off at 800' and have burnt rings around the bottom of the pots as well as blackened kiln shelves. Quote Link to comment Share on other sites More sharing options...
neilestrick Posted April 23, 2023 Report Share Posted April 23, 2023 35 minutes ago, SUZANNEHIG said: How did things turn out? I just had the same issue. I turned the kiln off at 800' and have burnt rings around the bottom of the pots as well as blackened kiln shelves. The wax and all the burn marks will burn out just fine if you let it run. If the smell is super bad then you'll want to explore better venting options. What type of vent are you using? Dale pots 1 Quote Link to comment Share on other sites More sharing options...
SUZANNEHIG Posted April 23, 2023 Report Share Posted April 23, 2023 2 hours ago, neilestrick said: The wax and all the burn marks will burn out just fine if you let it run. If the smell is super bad then you'll want to explore better venting options. What type of vent are you using? I Thanks for your response Neil. have a SKUTT Enivrovent that goes out the roof. Here is a photo of how bad it looks. The oval plate is turned over to show the burn ring on the kiln shelf. Quote Link to comment Share on other sites More sharing options...
neilestrick Posted April 23, 2023 Report Share Posted April 23, 2023 3 minutes ago, SUZANNEHIG said: Here is a photo of how bad it looks. Yup. That's what'll happen until it gets hot enough to burn all that out. There's not a lot of work in the kiln, so if the smell was really bad then your wax must be on pretty thick. Most wax resist can and should be thinned out before use. It only takes a very thin application to resist glaze. Quote Link to comment Share on other sites More sharing options...
Mark C. Posted April 24, 2023 Report Share Posted April 24, 2023 Next time let it go and all that will burn away-you got spooked and shut it down early. This will all be gone in a high fire-looks normal for an early cool shut off.Your smoke alarm should not be so close to this area Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted April 24, 2023 Report Share Posted April 24, 2023 @SUZANNEHIG Just in case you need this someday getting wax where you didn’t want it…. When a candle burns efficiently ya basically get carbon dioxide and water. When a candle burns inefficiently ya get lots of soot (carbon) which you found in your kiln. By about 800f the candle wax burns away and by about 1000f it’s basically gone. So if you want to burn unwanted wax off a piece and start over, you can fire to 1200f and be reasonably sure all traces of wax and carbon will be completely gone. Quote Link to comment Share on other sites More sharing options...
SUZANNEHIG Posted April 25, 2023 Report Share Posted April 25, 2023 Thank you everyone for all the feedback. Bill Kielb and Hulk 2 Quote Link to comment Share on other sites More sharing options...