I bought a used Bailey wheel. Used 5 times and then stored for 15 years.  It vibrates, especially at higher speeds. I knew at $200 and no belts it was a risk.

Any suggestions? It's not a wobble. The head rotates on a flat plane... But the vibration is pretty bothersome.

Thanks for your help!

Aminah

 

Link to comment
Share on other sites

If the head is spining flat-is the pully underneath bent? do the belts have flat spots on them from storage for 15 years? vibration usually can be seen-turn wheel on side and start it up and look around.

Link to comment
Share on other sites

aminah,   if you have any problem with a bailey product, you will not find a company more eager to help.   if the belt does not solve it,  call them and ask for a wheel tech.    do not send a text,  or email!     there is nothing as difficult as a one sided conversation.  have your wheel info handy to identify it and the tech will be able to give you the best solution to any problem.  

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.