Gin Posted March 15, 2021 Report Share Posted March 15, 2021 Hi, Any recipes for a stable white cone 6 satin white glaze that breaks on texture would be greatly appreciated something similar to maybe this examples I found on Pinterest Link to comment Share on other sites More sharing options...
Bill Kielb Posted March 15, 2021 Report Share Posted March 15, 2021 Have you ever searched Glazy.org? white, cone 6, oxidation : search https://glazy.org/search?keywords=White glaze&base_type=460&cone=30&atmosphere=1&photo=false&production=false Link to comment Share on other sites More sharing options...
liambesaw Posted March 15, 2021 Report Share Posted March 15, 2021 On my red clay this happens with every white glaze I've tried Link to comment Share on other sites More sharing options...
Gin Posted March 15, 2021 Author Report Share Posted March 15, 2021 Thank you Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted March 15, 2021 Report Share Posted March 15, 2021 Disclaimer: most white glazes will do this over dark clay, unless it’s a bit of a stiffer melt, or it’s got a really high amount of opacifier (more than 10%). I only mention, because Glazy has a pretty wide set of possibilities to choose from. Link to comment Share on other sites More sharing options...