  1. Hi, I am hoping to create an opaque semi matte/ satin glaze for dark clay body that is a warm rich brown copper with crystals…would this be RIO over 10% in a semi matte base or rutile and RIO or RIO and copper? fire to midrange cone 6 on stoneware oxidization with a slow cool for crystals to form ? will do testing but need some direction to get started please Thank you
  2. Thank you! will test and let you know.
  3. Hi, the recipe cone 6 lists light rutile, this is unavailable to me can I calcination rutile to get light rutile if so what temp and how long to hold? 1000F and hold 30 minutes? Thank you
  4. Thank you for your quick response sorry I was not clear… Minspar 200 Cheers
  5. Recipe is : M200 46.10 Silica 19.7 Gerstley 13.5 cal carb 8.20 dolomite 5.9 zinc oxide 3.9 can I substitute Custer Feld for M200 1:1 or do I need to adjust ? oxidization cone 6
×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.