jan goodey Posted October 9, 2020 Report Share Posted October 9, 2020 Hi, I'm looking to mimic rust on the surface of my pot. It should be matt. Can anyone help? Jan Link to comment Share on other sites More sharing options...
Babs Posted October 9, 2020 Report Share Posted October 9, 2020 Any photos to lead us? Link to comment Share on other sites More sharing options...
Sorcery Posted October 9, 2020 Report Share Posted October 9, 2020 I have a high iron, sandy red clay deposit I grab from that looks like rust between 6 and 10. This is it embedded into Standard 205 with slight reduction hot 9. It's more matte in oxidation, more shiny hotter and reduced. Sorce Link to comment Share on other sites More sharing options...
neilestrick Posted October 9, 2020 Report Share Posted October 9, 2020 What cone are you working at, and what type of kiln? Link to comment Share on other sites More sharing options...