effiep Posted April 29, 2020 Report Share Posted April 29, 2020 Hello, I bought a batch of Air drying clay nylon reinforced to do some pottery at home, but the clay appears to be too soft and muddy. I can't use a rolling pin or my hands for that matter to shape it and make things. Also it sticks everywhere. I tried adding water but it only makes it more slimy. Am I doing something wrong ? The label says it is supposed to be for modeling but this clay is like mud Link to comment Share on other sites More sharing options...
Babs Posted April 30, 2020 Report Share Posted April 30, 2020 Maybe ifyou listed the brand .country you are in help would flow. Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted May 1, 2020 Report Share Posted May 1, 2020 If it's too wet, adding more water won't help. You might try letting it set up for an hour before trying to use it if it's that mushy. Link to comment Share on other sites More sharing options...
Sorcery Posted May 9, 2020 Report Share Posted May 9, 2020 EffieP...you forgot the "u" in there! No worries, I effied Up my first go putting too much water too! Sorce Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.