Marilyn292 Posted January 4, 2020 Report Share Posted January 4, 2020 Has anyone had problems with rust forming in a stainless steel pug mill? Link to comment Share on other sites More sharing options...
neilestrick Posted January 4, 2020 Report Share Posted January 4, 2020 Stainless steel can rust. If you run a groggy clay through it it should clean it out pretty well. Link to comment Share on other sites More sharing options...
Min Posted January 4, 2020 Report Share Posted January 4, 2020 Haven't had any rust with my Bailey stainless mixer pugger. Link to comment Share on other sites More sharing options...
Mark C. Posted January 4, 2020 Report Share Posted January 4, 2020 Is this made by Skutt kilns-as I know they have poor stainless on other components??? Link to comment Share on other sites More sharing options...
Marilyn292 Posted January 5, 2020 Author Report Share Posted January 5, 2020 It’s a Peter Pugger SS . I just shipped it back to the company and am waiting for a response. This has been going on for almost 2 years. It started within the first six months of my ownership. I don’t use grogged Clay or use any abrasives. Just wondering if anyone else in the community has had similar problems. Link to comment Share on other sites More sharing options...
Mark C. Posted January 5, 2020 Report Share Posted January 5, 2020 What model # was it ? and tell us how this all turns out please. Thanks Link to comment Share on other sites More sharing options...
fergusonjeff Posted January 6, 2020 Report Share Posted January 6, 2020 I have had a SS Peter Pugger for about 5 years and used almost daily. Not a speck of rust or corrosion. I use some porcelain in my mix also. I am interested in hearing how your situation turns out. Link to comment Share on other sites More sharing options...