Wingnut Posted June 5, 2019 Report Share Posted June 5, 2019 New to ceramics and have a few questions. I currently have been working with ^04 bisque and ^06 glaze and low temp clay. I have lots of low fire clay and prefer to use up before getting any more. I mainly make large beads for macrame hangers. I am now making orchid hangers and want to know if the low temp clay unglazed will be a problem. I prefer for the hanger to hold some moisture much like a clay pot. I will also be glazing the edges and probably doing a decorative glaze stripe/coloring on the body leaving much of the hanger unglazed. My concern is low fire vs high . Pros and cons with any advise is trully appreciated. I have LOTS (100's) of orchids and wanted to make some different ways to display them. Link to comment Share on other sites More sharing options...
neilestrick Posted June 5, 2019 Report Share Posted June 5, 2019 Unglazed pots evaporate moisture much faster than glazed pots. So if you want to hold moisture in but have the look of an unglazed pot, just glaze the inside. Link to comment Share on other sites More sharing options...
Wingnut Posted June 5, 2019 Author Report Share Posted June 5, 2019 Is high fire clay stronger and more mold resistant than low fire clay? Link to comment Share on other sites More sharing options...
CactusPots Posted June 5, 2019 Report Share Posted June 5, 2019 High fire clay high fired absorbs very little water. If the orchid requires constant moisture and algae or mold is an issue, then glazing inside or out would help. My cactus and succulents prefer unglazed inside, I think. It's a great hobby to make pots specifically for your plants and watch how the different variables cause different growth. Link to comment Share on other sites More sharing options...
Mark C. Posted June 5, 2019 Report Share Posted June 5, 2019 low fire clay is not as strong as high fire wares Link to comment Share on other sites More sharing options...
Wingnut Posted June 5, 2019 Author Report Share Posted June 5, 2019 So would you say low fire is more porous therefore not as strong? Link to comment Share on other sites More sharing options...
liambesaw Posted June 5, 2019 Report Share Posted June 5, 2019 Definitely. More porous, unvitrified, however you word it, it's weaker. Link to comment Share on other sites More sharing options...
neilestrick Posted June 6, 2019 Report Share Posted June 6, 2019 Weaker, yes, but strong enough. Planters have been made from Terra Cotta for centuries. Link to comment Share on other sites More sharing options...
CactusPots Posted June 6, 2019 Report Share Posted June 6, 2019 Most terra cotta planters I have seen are much thicker than my stoneware planters. Neither one bounces, so strength is only a factor if you're dealing with root bound plants that can provide enough pressure to break the pot. I don't know orchids, but some succulents can do this. More to the point of high fire/low fire for planters is the watering schedule considering that the earthenware (terra cotta) will absorb water. Then you have to consider the other variables of planting media, environmental conditions, planter depth, and plant requirements. You're on the right track making your own pots if you're a serious plant collector. Link to comment Share on other sites More sharing options...
preeta Posted June 8, 2019 Report Share Posted June 8, 2019 Bisqueware at any temperature is fragile - whether earthenware or ^5/6 or ^10 claybody. because of its porosity. i would definitely experiment with earthenware just coz you have so much. you can use the principle of onggi potters. modern western ones who bisque and glaze fire but underfire the glaze and claybody so it remains porous but not as fragile as bisque. Could a vitrified earthenware be stronger than a cone 10 body glaze fired to cone 6? Link to comment Share on other sites More sharing options...