Marge Posted September 5, 2018 Report Share Posted September 5, 2018 I've been reading past posts regarding the safety of using Barium Carbonate in a glaze. I understand the dangers to the potter while making the glaze, I use every precaution possible. Should I feel comfortable using it in mugs and dinnerware? My recipe calls for 9%... Thanks... Link to comment Share on other sites More sharing options...
neilestrick Posted September 5, 2018 Report Share Posted September 5, 2018 No, I wouldn't use it at all in functional ware. Link to comment Share on other sites More sharing options...
Mark C. Posted September 5, 2018 Report Share Posted September 5, 2018 You can use it on the outside of wares not inside or the lip. Its best on nonfunctional wares. Precuations need to be had when handling it as well 9% is lot Link to comment Share on other sites More sharing options...