kraythe Posted November 8, 2017 Report Share Posted November 8, 2017 Apologies for the thread spam but I have another question for you experts. I currently have glaze recipes that call for silica 200 mesh but I only have 350 mesh and I was wondering if that is a valid substitute or if I will be messing the glaze up. So what effect will the smaller mesh size have and does it really matter? Link to comment Share on other sites More sharing options...
High Bridge Pottery Posted November 8, 2017 Report Share Posted November 8, 2017 You're probably better off using 350 mesh anyway, I am not sure how much of a noticeable difference there's between the two, I think you could probably guess that it might 'look' like you fired 200 mesh silica half a cone hotter by using 350 mesh as the smaller particles will melt easier. Link to comment Share on other sites More sharing options...
kraythe Posted November 8, 2017 Author Report Share Posted November 8, 2017 thanks. Link to comment Share on other sites More sharing options...
Mark C. Posted November 8, 2017 Report Share Posted November 8, 2017 Glaze will melt better with your 325 silica over the 200 silica.Never heard of 350-maybe its an over the pond deal? Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.