lamsteven7 Posted April 27, 2016 Report Share Posted April 27, 2016 Hi everyone, I have seen this pot and do not how to make it. can u help me to identify it . Link to comment Share on other sites More sharing options...
cloudhutworks Posted April 27, 2016 Report Share Posted April 27, 2016 Is this even a clay pot? Looks like concrete with paint and various inclusions to me... But if it ceramics I too wonder how to make one Link to comment Share on other sites More sharing options...
neilestrick Posted April 27, 2016 Report Share Posted April 27, 2016 Looks like a crater glaze that has been sanded down. Add some silicon carbide to a cone 6 glaze and it can cause bubbling. After the firing, grind down the bubbles and sand them smooth. Link to comment Share on other sites More sharing options...
oldlady Posted April 27, 2016 Report Share Posted April 27, 2016 there are lava glazes that give that effect. Link to comment Share on other sites More sharing options...
bciskepottery Posted April 27, 2016 Report Share Posted April 27, 2016 Crater or lava glaze that might have been sand-blasted post firing. Link to comment Share on other sites More sharing options...