MFP got a reaction from Hulk in Vertical stripes
Thank you both for your advice. I appreciate it. For some reason I am having trouble responding to the posts. Hulk-- the tip about not letting it get too dry makes a lot of sense.y studio is like a sardine can with the sardines in it -- so no room for spraying. Thanks again
-
MFP got a reaction from Callie Beller Diesel in Mayco Indigo Rain
If anyone uses Mayco Indigo Rain and has noticed how dry and rough it's become since they changed the talc-- and it won't melt with Splatterware anymore no matter how hot you get it--- the fix is adding 25 grams of gerstly borate to a full container of glaze. It restores the previous smooth surface and it melts with Splatterware again.
-
MFP got a reaction from Min in Mayco Indigo Rain
If anyone uses Mayco Indigo Rain and has noticed how dry and rough it's become since they changed the talc-- and it won't melt with Splatterware anymore no matter how hot you get it--- the fix is adding 25 grams of gerstly borate to a full container of glaze. It restores the previous smooth surface and it melts with Splatterware again.
-
MFP got a reaction from Bill Kielb in Propane hook up for Olympic 2831 kiln
Thanks so very much Bill!
Marie
-
MFP got a reaction from MamaJenXO in Underglaze Bleeding Wanted!
I just had a cone 6 fire where I put Amaco undeglaze on the top of a glaze.....it did blend in better....it was on top of Amaco Snow Celadon. I tried the white on Amaco Mulberry celadon and it did not entirely melt.