Chances are the body bands have loosened and the hinge has dropped a little bit as a result. You'll need to reset the hinge. Remove the tension on the lid spring, loosen the screws holding the hinge plate, then adjust the body bands if they have sagged and tighten them all up. Then push up the hinge so it's in the correct position with the main hinge rod sitting in the bottom of its holes and tighten the hinge screws. Then set the spring. I would also add a latch to the front of the lid to help keep it shut
-
That's a big gap. Does the lid sit totally flat at room temp, or is it hitting at the back edge?
-
Mishima with soy based wax resist
neilestrick replied to Catwings's topic in Clay and Glaze Chemistry
Yes, I use a needle. You have to let the burrs dry for a bit before brushing them off or they'll just smudge back into the lines.- 10 replies
-
- mishima
- wax resist
-
(and 1 more)
Tagged with:
-
It's not just a Skutt thing. Kiln power wires wear out and must be replaced at some point.
-
Error8 message on E23 Cress kiln
neilestrick replied to terraworks57's topic in Equipment Use and Repair
What is error 8 on that controller? This one?: In CONE FIRE mode, the temperature is falling in the last segment instead of increasing. It could be because of a power outage, but it could also be a relay sticking when it gets hot. If it's a relay, it'll probably totally fail soon. Were there other signs of power outage in your building- clocks flashing, etc? -
Hot spots at the elements connections don't cause the relays to fail, they just cause that connection to fail. There's no safe way to get access to a Skutt relay while it's under load, due to the way the box is constructed. You just track the number of firings you have on a set of relays, and if they're burning out under 150 firings then you replace the wiring harness and it's good to go.
-
It was the old wiring. I've literally seen it dozens of times. Even Skutt recommends replacing the harness if relays are burning out prematurely.
-
@Caroline Ennis One of the best features of the Skutt and Bailey wheels is the large splash pan. It keeps the studio much cleaner.
- 12 replies
-
- pottery wheel
- shimpo
-
(and 3 more)
Tagged with:
-
The top and bottom sections do not have the same 2 elements in them. The 1231PK has 2 top/bottom elements, 2 intermediate elements, and 3 center elements. So top and bottom sections each have 2 different element in them- T/B and intermediate. They're wired with crimp connectors, so you can't unhook them, which is why Skutt only publishes the resistance of each section, not of each element.
-
@Lilith Rockett I would still like you to check the temperature of the power wires when the kiln is reaching its peak temp. I assume you have a disconnect box by the kiln? Open that up and see if the wires are hot in there. Also feel the whip everywhere from the kiln to the disconnect and see if it's getting hot. Also check your breaker and see if it's running hot.
-
Mishima with soy based wax resist
neilestrick replied to Catwings's topic in Clay and Glaze Chemistry
I use the wax from Ceramic Supply Chicago, and it works fine as long you don't let it dry too long, like don't let it sit overnight. It also depends on how soft the clay is. Too dry and the clay will flake, too. I typically apply the wax and then cut my lines as soon as it's dry to the touch.- 10 replies
-
- mishima
- wax resist
-
(and 1 more)
Tagged with:
-
I have 9 Skutt wheels, and love them. Their 1/3hp models can handle just about anything you would want to make.
- 12 replies
-
- pottery wheel
- shimpo
-
(and 3 more)
Tagged with:
-
Brand new dual input pyrometer not working
neilestrick replied to MIsty's topic in Equipment Use and Repair
Is it in a very cold environment, like a garage? It could be that the pyrometer is not able to read below a certain temp. Also check that the two wires are connected to the correct ends of the thermocouple, red wire to the red end. -
Brand new dual input pyrometer not working
neilestrick replied to MIsty's topic in Equipment Use and Repair
@MIsty Can you post a picture of it? What brand is it? -
The controller cycles the SSR's twice per second (500ms). When I put a meter on mine it gives a fluttery reading. @Lilith Rockett This is a long shot, but 3 times in the last 20 years I had kilns similar in size to yours have a very strange stalling problem. It turned out to be an electrical interference issue (there are a lot of magnetic fields and whatnot created by the elements and bricks), and the solution was to make sure the controller was directly grounded, not just through the transformer. It's an easy fix and worth trying if yours isn't already grounded that way. Take a look at the backside of your controller, there needs to be a wire that goes directly from the Center Tap terminal to the grounding stud. Not to the transformer or anywhere else first. You may need to get a terminal doubler so you can add another wire.
-
Rewiring A Duncan Energy Saver, The Teacher kiln
neilestrick replied to AddisonSedergren's topic in Equipment Use and Repair
There's nothing more or less safe about 3 wire vs 4 wire. It just depends on the needs of the kiln. Having a ground is the real safety issue, which you do. As Dick said the kiln needs to be on a circuit that is 125-150% of the draw of the kiln. I think your kiln draws around 24 amps? Check the serial plate to confirm, but if that's the case it should be on a 30 amp breaker. -
I always liked that type of connection. Simple and solid. It was fairly common a long time ago, but nobody uses it anymore.
-
@JohnnyK I just had a nice conversation with Steve at L&L, and he confirmed what I said above. The non-twisted end will not heat nearly as much as the coils inside the kiln do. For one, the coils feed off each other and run hotter- this is why they get hot spots when they bunch up at the corners. Plus the coils are in an insulated environment, whereas the end can dissipate heat fairly well, assuming the control box has good air flow. That said, there are a couple of things that may be an issue with your Cress compared to the L&L. First, the L&L element connection has a much greater surface area in the connection by using bolts, nuts, and washers. Plus all of that hardware is stainless steel, which is more durable and won't expand and contract as much as brass or copper connectors. The second potential issue is frying out the feeder wires if they're pressed up against the element connections when you close up the box. The L&L control box design directs the wires away from the connections so it's not an issue with their kilns. At this point I don't think there is really anything you can do besides fire the kiln and see what happens, but I think there's a good chance it will be fine.
-
Some more info on non-twisted ends HERE. I'll have more info on this later today. I'm going to see if there's something about the L&L element connection system that makes non-twisted ends more viable than other element connection types (crimp, screw). There is no difference in element life between the twisted and non-twisted in L&L kilns. They are not more likely to burn out at the element connections or through-hole or anything like that.
-
@Lilith Rockett Have you had the service wiring checked out? I had a customer once where everything on the kiln checked out just fine- element resistance was dead on, thermocouples and relays were new, etc, but it kept erroring out at higher temps. Turns out the outlet and power cord were heating up and affect the draw once the kiln had been running for several hours and getting up to higher temps. Also, that kiln was kinda buggy from the beginning and really burned up relays fast, so we isolated the controller from the main power with its own 120 volt plug, and that fixed the bugginess.
-
L&L does not twist the ends on a lot of their elements, especially the beefy ones. The elements on my eQ2827-3 are not twisted, and they do not glow when the kiln is firing. I think that a straight wire does not heat the same as the coiled wire, which makes sense because I know that coil density is one of the factors in element design. I've sent an email off to L&L to get more information on this, but for now I would say that @JohnnyK your elements are going to be fine. The resistance difference is not going to be an issue at all.
-
Including a new controller and relays? Have you put a meter on the elements while the kiln is firing to verify that they're getting power? Checked voltage and amperage draw of the middle section under power? S and K type thermocouples being wrong should result in much bigger issues than this. Thermocouples being connect to the wrong sections should result in a pretty quick error, as the sections will heat much too quickly.