I just got back from 3 days/2 nights of free studio time from the Mendocino Art Center (CA). I've sold in their gallery and taken many workshops there and they heard about the loss of my house/studio, so they offered me this wonderful gift. It was the first time since the fire that I've worked with clay and it felt fabulous!! Someone was firing a ^6 kiln and was able to fit a few of my shards in, and they refired beautifully, so I'll refire a lot of my other shards so I...
-