Right now several months' glazed work is in the big and small kiln. I need to fire smaller loads, and more frequently!
-
Exciting!
-
Remember the famous saying: "Fire first and ask questions later." Okay, not so famous, I just made it up.
-
LOL! I had mostly good results. A couple of my new dipping glazes are a bit thick so I'll adjust them but nothing is ruined. My dad insisted on firing at Cone 6 which my Cone 5 glazes did NOT like; I had a couple glazes drip that have never dripped before. Otherwise a successful glaze load!
-