Single Status Update
-
Working madly on glazing two loads of bisque. I'm starting to really regret all the plans I had for iron oxide because it's a pain to work with!!
- Show previous comments 2 more
-
Weird, it cut off the comment.
I end up with horribly stained palms, wrists and nails for about three days no matter how much I scrub.
-
Yuppers.
-
Weird! I have micaceous redart and another terracotta, but my hands don't stain. That must be some serious red clay!!
- Show next comments 3 more