Disappointed (with emphasis). When you open the kiln excited to see vibrant colours on decals (12 pieces) and what you actually get is grey on white.
- Show previous comments 2 more
-
Maybe my decals are different. I fire them to 017 which is around 1300 F. Are you working with degrees Centigrade?
Good job on making lemonade out of lemons!
-
Yes I fire to cone 8 1260 Celcius.
-
Maybe your decals are different than mine, but the 3rd firing I do for decals is at a much lower temp. Perhaps that is why yours lost all their color? I found Milestone decals to have a wealth of information about application and firing. I think they also have some youtube videos.
Roberta