MIXED MY FIRST GLAZE TODAY! EVER!
- Show previous comments 1 more
-
I will feel more magical when I get the results out of the kiln later this upcoming week. I will fire it tomorrow. I think one of them is a bit too thick. So only time will tell. But it was easier than I thought it was to mix the stuff together, at least a test batch of 400G.
-
post the results.
-
Where at? In my gallery?