Silicon Carbide is arriving today. Going to mix up some test batches of some reduction glazes to experiment in oxydation chemically reduced! Lots of terrible glazes to come!
- Show previous comments 1 more
-
I am firing 3 test right now in a slightly different schedule with a hold on the way up to burn out some gasses. I will post the results if they are anything decent in the tenmoku thread.
-
I have tried walking down this road. Results when you get them: good, bad, or indifferent.
-
You did some silicon carbide stuff? What did you try?
- Show next comments 9 more