  1. Firing over 200 test tiles in the next few days over 4 glaze firings. Normal Slow Glaze ^6, Slow Glaze ^5+1Hour Hold, Slow Glaze ^6 + slow cool, Slow Glaze ^6 super slow cool. Want to see all the variants of the same glazes and how they behave differently. Should be interesting.

    1. Show previous comments  9 more
    2. Joseph Fireborn

      Joseph Fireborn

      2nd kiln load coming out in a few hours. I will have pictures comparing the two and I will post a like to a photo bucket of each tile .. over 70 so far.

    3. Joseph Fireborn

      Joseph Fireborn

      So unloaded the 2nd firing. I am haven't compared tile to tile yet, but I found some new discoveries I am very very happy about! Like pee my pants happy. One thing I noticed is that most of the glazes are very similar to the straight cone 6 firing, except that the surface of the cone 5 + 50 minute hold had a much better surface. Less defects. I went past cone 6 a little though about 6.5 probably.

    4. Joseph Fireborn

      Joseph Fireborn

      Posted pictures of the glaze tiles I will probably work with in 2016.