Drove 60 miles to pick up some Wollastonite, could not get rid off bubbles from Whiting or Dolomite. Be funny if I open the kiln and there are still bubbles >;(
-
not sure how bad your bubbles are, but I sometimes squirt diluted alcohol which breaks the surface tension of the bubbles...at least the ones floating on top. I learning this from plaster mixing with Richard Notkin who learned it from professional mold makers. It does not have any effect on the glazes.
-
Thanks for the tip Marcia but this isn't to do with application issues. Will try it next time I am making plaster moulds My problem is with the LOI leaving bubbles in my fired glaze.
-
when i sub wollastonite for whiting/silica the glazes flux more when the formulas are balanced. i need to slightly undersupply the calcium part of the original formula.
-
-
Having a dabble into changing firing schedules to get rid of bubbles. Tried a slow cool with no luck, still just as many. Tried a hold at 900c for 20 mins after reading that is the temp dolomite and whiting have finished gassing. Excited to see if that has made any changes.
- Show previous comments 3 more
-
That's what I was trying with the hold at 900c. Didn't seem to make much difference. Going to put a ball of glaze in my bisque and see if it has already started melting.
-
Can you get wollastonite where you live? Since whiting has approx 45% loi lots of gassing out that has caused problems with some of my glazes before i rejigged recipes. doesn't always work but sometimes it did the trick.
-
If I can't solve the problem I will have to buy some wollastonite. Just been trying to use what I have in the stores.
-
Working night shift with the super moon eclipse. Should be great viewing with the clear sky up the north of England.