I mixed clay today! Picked up dry clays about 11, did errands, and started mixing about 1 pm while the sun was warm . Cold front is coming in tonight. Beat it! So happy. Mixed about 270 pounds wet. That should be a good start. This batch is for making new saggers. I didn't bring many with me. My birthday is Wed. so I can celebrate by doing some throwing. Kilns will be getting wired in Mid- February.
-
Early Happy Birthday Marcia. Mine is the following wednesday. Aquarius rules. LOL. Hope the day will be filled with sunshine on Wednesday for you. Don't fire the cake, fire the kiln.
-
Happy Birthday to you too. It is snowing-dumping. Waiting til it ends to shovel, but they say 3 days.