The tree images on these Cityscape bottles are what the HP Laserjet decals look like once they are fired to cone 6 (oxidation). The slide-off decal paper came from: Decal Paper, 12610 NW 1115th Ave. - Bldg 200, Medley Florida 33178. The printer that I used is an old HP LaserJet4000TN...ink from this printer includes enough iron that it fires very well onto previously glazed surfaces.