From the album: LaserJet Decals
The tree images on these Cityscape bottles are what the HP Laserjet decals look like once they are fired to cone 6 (oxidation). The slide-off decal paper came from: Decal Paper, 12610 NW 1115th Ave. - Bldg 200, Medley Florida 33178. The printer that I used is an old HP LaserJet4000TN...ink from this printer includes enough iron that it fires very well onto previously glazed surfaces. -
From the album: LaserJet Decals
The tree images on these Cityscape bottles are what the HP Laserjet decals look like after the decals are printed, cut out, soaked (briefly), and slid onto the previously glazed surface. At this point in th eprocess, the images are black. The slide-off decal paper came from: Decal Paper, 12610 NW 1115th Ave. - Bldg 200, Medley Florida 33178. The printer that I used is an old HP LaserJet4000TN...ink from this printer includes enough iron that it fires very well onto previously glazed surfaces.