glazenerd 1,644 Posted April 15, 2020 Report 1. Hematite. 2. Pure clay( no additions) hematite. 3. Hematite with 3% TiO2 added. 4. Magnetite 5 Newman Red. 6. Red Art. All samples fired in oxidtion. Quote Link to comment
JohnnyK 723 Posted April 16, 2020 Report The great takeaway from this experiment is that it is of paramount importance to know what color the clay is going to be at the final firing so that you have a better idea of how to go about glazing the pieces since their final color will be affected by the base color of the clay at cone... Thanks, nerd! Quote Link to comment
glazenerd 1,644 Posted April 16, 2020 Report Johnny: yes, that is part of the equation. Several other parameters I am going to test as well. Glaze interaction with iron is on the table currently. Quote Link to comment
Joseph Fireborn 1,369 Posted April 29, 2020 Report Number 2 at cone 6 is a remarkable color. Beautiful Quote Link to comment
Recommended Comments
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.