JohnnyK 975 Posted April 25, 2019 Report Share What glazes & application methods did you use to achieve such a fantastic result? Quote Link to comment
dhPotter 472 Posted April 25, 2019 Report Share Hey JohnnyK, Around the rim, where the glaze is lighter, is Strontium Crystal Magic Cool sprayed on. Then Pete's Seafoam is sprayed over the whole piece. The SCMC makes Pete's Seafoam go turquoise. Depending on thickness of Pete's Seafoam, on non-SCMC areas, will result in the varied amount of splotches. The army green color is where Pete's Seafoam is thinner. Thank you JaneyD and LeeU 2 Quote Link to comment
Joseph Fireborn 1,447 Posted April 27, 2019 Report Share nice spray work. really can tell the time you put into learning the spray gun and glaze methods. dhPotter and JaneyD 2 Quote Link to comment
JaneyD 0 Posted May 3, 2019 Report Share My first time on here this morning and what a beautiful glaze! Not sure what Pete’s Sea Foam is but it is a lovely colour Quote Link to comment
dhPotter 472 Posted May 3, 2019 Report Share Thank you all for your kind words. Joseph, as you know, it takes time to sort out the glazes and how to apply each one. Pete's Seafoam is a glaze recipe created by Pete Pinnell. Quote Link to comment