JohnnyK 688 Posted March 28, 2019 Report Great concept...is the dip bowl affixed to the platter? Quote Link to comment
dhPotter 431 Posted March 28, 2019 (edited) Report Thank you, JohnnyK, yes it is. Glazed the platter then set the bowl on it to glaze fire. I'm thinking to get a better seal would be to put a little glaze on the bottom of the bowl also. There isĀ 1 spot between bowl and platter where you can almost put a fingernail into. Edited March 28, 2019 by dhPotter Quote Link to comment