JoLinDesigns Posted September 5, 2014 Report Share Posted September 5, 2014 Is there any way to salvage a glazed piece where a witness cone melted on it! Link to comment Share on other sites More sharing options...
Mark C. Posted September 5, 2014 Report Share Posted September 5, 2014 You could grind it off and reglaze and refire-thats about it and it will never look the same refired. Mark Link to comment Share on other sites More sharing options...
JoLinDesigns Posted September 5, 2014 Author Report Share Posted September 5, 2014 Yeah. That's what I was thinking. Thanks! 4 tiles fired 3 times and perfect. Then this!! Not my week!! Link to comment Share on other sites More sharing options...
Babs Posted September 5, 2014 Report Share Posted September 5, 2014 Goes with the field, think yo've got it then something different happens, exciting! Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.