Becca Posted December 12, 2013 Report Share Posted December 12, 2013 Hi all! I would very much appreciate any advice on my small quandary: I let a friend make a few bowls as a Christmas present for his wife, and I was planning/hoping to throw them in with the low fire (^06 ) glaze firing I have already planned. Being that he used a ^6 clay body, bisque firing them to ^06 seems permissible, although I usually do bisques at ^08. However, reading up on the question, I discovered that it is not a good idea to mix greenware and glaze ware in the same firing, even if they require the same temperature, do to the possibility of gasses produced by the greenware interfering with the glaze chemical reactions. My question is this: how bad of an idea is it to do it anyway, being that all of my pots are glazed in a clear glaze with black and white underglazes?? He needs them by Christmas of course, and I do not have any additional greenware to fire at the moment. So ya see, I was hoping to save dollars (and greenhouse emissions) by not having to do an entire bisque firing for four bowls... Advice from all you smart potters out there would be very appreciated!! Thank you! Link to comment Share on other sites More sharing options...
Benzine Posted December 12, 2013 Report Share Posted December 12, 2013 Firing both together should not be an issue. To avoid any potential issues from the bisqued items off gasing, just don't pack them very close, to the other glaze items. Just make sure that the greenware bowls are completely dry. There's nothing worse than fining glazed pieces with chunks of bisqueware fused into them, from exploded wares. It's the main reason I don't fire both together in my classroom kiln. Everytime I decide to try, something that I thought was dry, had a thick spot I didn't know about and....disaster. Link to comment Share on other sites More sharing options...
Becca Posted December 12, 2013 Author Report Share Posted December 12, 2013 Thank you!!! Great news! Link to comment Share on other sites More sharing options...
Mudslinger Ceramics Posted December 13, 2013 Report Share Posted December 13, 2013 Hi Becca I have fired glaze and bisque together occaisionally too and except for the first time all is well. Had one pot blow out because I set the firing schedule to suit the glaze ware but thankfully no damage to other pots. The beginning of the firing must be set for the benefit of the bisque so that all the chemical water is driven off slowly first, then the last part of the firing must suit the glaze so that there is time for the heat to even out in the kiln and mature the glaze....adds about 2-2.5 hours to my regular glaze schedule. Also stack my bisque on the lower shelves so that if all the heatwork falls short then the glazes are not affected and it doesn't change much of anything for the bisque, also stacked this way any blowouts won't rain down on the glaze ware either. Good luck. Irene Link to comment Share on other sites More sharing options...
Becca Posted December 15, 2013 Author Report Share Posted December 15, 2013 Thank you for the tips, Irene and Norm! Very thorough advice that will be well heeded. And Norm, regarding your comment about bisque firing temps: I fire at ^08 because its how I learned in school. I haven't had my own studio for long, so I am still stuck in this steep learning curve- always so much to learn in this field. I HAVE been having issues with pin-holing and crazing.... Perhaps I need to be bisquing at a higher temp?! Thank you for the advice. Link to comment Share on other sites More sharing options...
clay lover Posted December 16, 2013 Report Share Posted December 16, 2013 Becca, I went from bisquing at 06 up to almost ^04 . I do 1920 with a 20 minute hold for my kiln. That solved many problems. glaze goes on smoother with dipping, and most all pinholing stopped. Ask your clay supplier what their clay needs, they should know. Link to comment Share on other sites More sharing options...
TJR Posted December 16, 2013 Report Share Posted December 16, 2013 I bisque at cone 06 all the time. I normally would bisque at 07 ,but I am out of those cones and have lots of 06's. Unless you are experiencing pinholing, you don't need to fire any hotter. TJR. Link to comment Share on other sites More sharing options...
Chris Throws Pots Posted December 18, 2013 Report Share Posted December 18, 2013 Hi Becca, Why not just load the four bowls at the bottom and shelf over them. It would be a waste of some space, but certainly nowhere close to firing the four bowls by themseves. This way, even if there was an explosion, the glazed wares would be shielded by the shelves. This would definitely give enough distance so that gas interaction would not be of issue. Good luck, Chris Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.