Chris Campbell    1,087

Neil is right ... You will either under fire the clay or over fire the glaze.

Under fired clay is weak and over fired glazes crack and/or run.

 

However ... It all depends on what you want to do and how you want to do it.

If you love the glaze color and can't get it any other way then you have to adapt.

You could fire the clay to its temperature of Cone 6 then glaze it and re fire to Cone 04-06

If it were a sculpture or other non functional object you could just glaze and fire the whole thing cooler ... Maybe not as low as Cone 04 ... you might try higher temps to see what happens. Maybe Cone 2, 3 or 4? Put it on something so if it runs you won't have a shelf to clean.

Share this post


Link to post
Share on other sites
Iforgot    2

Neil is right ... You will either under fire the clay or over fire the glaze.

Under fired clay is weak and over fired glazes crack and/or run.

 

However ... It all depends on what you want to do and how you want to do it.

If you love the glaze color and can't get it any other way then you have to adapt.

You could fire the clay to its temperature of Cone 6 then glaze it and re fire to Cone 04-06

If it were a sculpture or other non functional object you could just glaze and fire the whole thing cooler ... Maybe not as low as Cone 04 ... you might try higher temps to see what happens. Maybe Cone 2, 3 or 4? Put it on something so if it runs you won't have a shelf to clean.

 

 

 

Smart, Smart

Share this post


Link to post
Share on other sites
oldlady    1,323

gypsy, your title suggests that you might think that cone 06 is hotter than cone 04. the reverse is true. maybe i am misreading you or maybe i have always assumed that whenever anyone talks about a range of temperatures the lower number is mentioned first. from low to high.

Share this post


Link to post
Share on other sites
Nat    0

I often use earthenware glazes on a stoneware body...sometimes it crazes, sometimes not...I happen to love the crackle effect though, but if you're glazing items that need to be food safe, it's not so good.

Share this post


Link to post
Share on other sites
Claypple    29

The answer depends on what Gypsy is making and what glaze she is using.

 

Chris is right, re-firing up to ^6 and then glazing at ^06 probably is the most common solution.

Share this post


Link to post
Share on other sites
gypsy    0

Thanks everyone. I have cone 6 clay and wanted to fire mayco specialty glazes but didnt know if it would work.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×