Any helpful drying hints?

Recommended Posts

Pugaboo    438

I just finished my first piece that I made on my own and now don't quite know the best way to dry it so it doesn't crack. In class at the end of the day the teacher asks us if we are done and if we are he covers it in plastic and sets it on a shelf. When we come back to class the next week they are all miraculously drying or dried and ready for the next step. I have noticed that the plastic seems to be in a different positions or state when we get to the next class so he must be doing something to help them dry properly yes? Soooo what magic is he doing while we are not looking? I finished a large cooking utensil holder here at home and it is currently sitting on and wrapped in plastic in preparation for drying. Do I just leave it wrapped up? If so for how long? Do I slowly remove the plastic over so many days? I have attached a picture so you can see what the item looks like since I know that may help in any suggestions given.

Thank you in advance for your help.

post-22921-136234751745_thumb.jpg

post-22921-136234751745_thumb.jpg

Share this post


Link to post
Share on other sites
bciskepottery    925

Let it dry slowly. I'd keep the whole thing under plastic the first day to allow the moisture in the clay to even itself. Then, unwrap but keep plastic over the top third . . . the bottom is thicker and moisture will go towards the bottom due to gravity; keeping the top under wraps allows the moisture to evaporate more evenly. Keep it in a place where the temperature is even and consistent. Let the pot dry on its time, not someone else's. This is the part where you learn patience is your friend.

Share this post


Link to post
Share on other sites

Turning my pots upside down, I let them dry uncovered during the day and then cover them each night.

This will extend the drying time several days in my case.

 

 

smile.gif

Share this post


Link to post
Share on other sites
Davidpotter    8

I just finished my first piece that I made on my own and now don't quite know the best way to dry it so it doesn't crack. In class at the end of the day the teacher asks us if we are done and if we are he covers it in plastic and sets it on a shelf. When we come back to class the next week they are all miraculously drying or dried and ready for the next step. I have noticed that the plastic seems to be in a different positions or state when we get to the next class so he must be doing something to help them dry properly yes? Soooo what magic is he doing while we are not looking? I finished a large cooking utensil holder here at home and it is currently sitting on and wrapped in plastic in preparation for drying. Do I just leave it wrapped up? If so for how long? Do I slowly remove the plastic over so many days? I have attached a picture so you can see what the item looks like since I know that may help in any suggestions given.

Thank you in advance for your help.

 

 

I never use plastic unless its really thin or if there is a possibility of warping. though sometimes the room is a little too dry and i one will crack.

Share this post


Link to post
Share on other sites
Pugaboo    438

Reading your suggestions I am wondering if moving it into a drying cabinet that I have that has wire shelves in it would be helpful. It's the size of a small refrigerator but not air tight, got it from a hospital when they closed down their old ex-ray lab and went digital instead; they used it to dry the big sheets of ex-rays. I don't have to turn on the fan or heater but it would be in a controlled environment that should (I think) give it a stable air environment to dry in and the shelf should allow air around it 360 degrees. Do you think I should still turn it upside down to dry? Won't the wire shelves leave indents across the top edge? It might take a little longer to dry in the cabinet due to limited air flow but again going by your suggestions slower is better yes?

 

Thank you for the suggestions I really appreciate you taking the time to help a beginning potter.

 

Terry

Share this post


Link to post
Share on other sites
Mark C.    1,798

We drape all handle production with thin plastic for 1 night. The best is those thin bags from like a dry cleaners-cut open in sheet form.

Also used a bunch of the thin plastic from store Banana boxes as it has some small holes so it slows but does not stop the drying process.

 

Mark

Share this post


Link to post
Share on other sites
Denice    243

Metal racks can leave pressure marks that might show if your using clear glaze, I have never chip or dented my pieces in my drying cabinet. Have you used this cabinet before? My first cabinet was an old refrigerator it was too tight, my second one was plastic shelves wrapped in plastic, too fragile. Third one in a plastic utility cabinet with adjustable shelves and already vented, it works perfect, I put old refrigerator racks on the shelves so the clay doesn't sit on plastic and had better air flow. Denice

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×