Posted 05 May 2012 - 12:13 PM

We are a group of 4 ceramicists that share a huge 600 sq meter studio in our city. At meetings we always complain that we never have time to make 'new' stuff. Growing our portfolio of work. There is always orders to complete, kilns that crash, etc.

Anyway, we decided to have these little 'pressure' tests. Once a month we will draw a project out of a bag. By mid month we have to have the item dry and ready for firing. End of the month we each have to show a new prototype. This could be included in our product range, and be beneficial to us all. But by having a little 'contest' we are all forced to make something new every month.

I decided to start a blog about this project. If you want to read about us and it: http://theclaycollective.blogspot.com/
Diana
www.dianaferreiraceramics.com
https://www.facebook...70824173&type=3

#2 StefanAndersson

StefanAndersson

    Member

  • Members
  • PipPip
  • 24 posts

Posted 05 May 2012 - 01:02 PM

We are a group of 4 ceramicists that share a huge 600 sq meter studio in our city. At meetings we always complain that we never have time to make 'new' stuff. Growing our portfolio of work. There is always orders to complete, kilns that crash, etc.

Anyway, we decided to have these little 'pressure' tests. Once a month we will draw a project out of a bag. By mid month we have to have the item dry and ready for firing. End of the month we each have to show a new prototype. This could be included in our product range, and be beneficial to us all. But by having a little 'contest' we are all forced to make something new every month.

I decided to start a blog about this project. If you want to read about us and it: http://theclaycollective.blogspot.com/

Great idea!

#3 INYA

INYA

    Advanced Member

  • Members
  • PipPipPip
  • 87 posts
  • LocationSlovenia, Europe

Posted 05 May 2012 - 05:10 PM

great idea, really!

I will follow the blog...
.......................

skratblog.blogspot.com
www.skrat.eu

#4 smokin pots

smokin pots

    Advanced Member

  • Members
  • PipPipPip
  • 124 posts

Posted 05 May 2012 - 09:40 PM

Count me in as well! I can't wait to see what y'all create.
juli
la paloma texas pottery

#5 Diana Ferreira

Diana Ferreira

    opinionated ignoramus

  • Members
  • PipPipPip
  • 186 posts
  • LocationCape Town, South Africa

Posted 08 May 2012 - 01:25 PM

We have uploaded another entry on the blog. There has been much action behind the scenes, and lots of discussions in the studio. The consensus is that our little test to come up with new work is actually working. The probable June project was discussed today!
Diana
www.dianaferreiraceramics.com
https://www.facebook...70824173&type=3

#6 trina

trina

    Advanced Member

  • Members
  • PipPipPip
  • 437 posts

Posted 08 May 2012 - 01:32 PM

That is another super good idea! I will definately follow the blog... T

#7 Diana Ferreira

Diana Ferreira

    opinionated ignoramus

  • Members
  • PipPipPip
  • 186 posts
  • LocationCape Town, South Africa

Posted 18 May 2012 - 01:54 PM

Some new images and entries to our blog. The heat is definitely on. And a bit of friendly rivalry is not a bad thing :-)

http://theclaycollective.blogspot.com/
Diana
www.dianaferreiraceramics.com
https://www.facebook...70824173&type=3

#8 Heidi

Heidi

    Member

  • Members
  • PipPip
  • 27 posts
  • LocationCape Town, South Africa

Posted 21 May 2012 - 05:50 AM

This is so interesting. Can't wait for the finals!



#9 Karen B

Karen B

    Potter 1981-present

  • Members
  • PipPipPip
  • 209 posts
  • LocationMassachusetts

Posted 21 May 2012 - 07:56 AM

Some new images and entries to our blog. The heat is definitely on. And a bit of friendly rivalry is not a bad thing :-)

http://theclaycollective.blogspot.com/






I Love Karen's. Simple and beautiful.

#10 Diana Ferreira

Diana Ferreira

    opinionated ignoramus

  • Members
  • PipPipPip
  • 186 posts
  • LocationCape Town, South Africa

Posted 21 May 2012 - 11:16 AM

I will tell her, Karen. Things are a bit slow now - drying and bisque firing. I will add more posts in a few days, as soon as stuff is happening again.