Posted 30 April 2012 - 01:11 PM

Somewhere I've seen a video of someone (Sandi Pierantozzi?) making interesting pot bottoms with 3 feet by folding in three sections. I can't find it on line. Does anyone know what I'm talking about? Where can I see how to do it??

#2 Matt Oz

Matt Oz

    Advanced Member

  • Members
  • PipPipPip
  • 308 posts
  • LocationMichigan

Posted 30 April 2012 - 01:20 PM

Here is the link

Handbuilding Video: How to Make a Textured Tripod Po

#3 Juli Long

Juli Long

    La Paloma Texas Pottery

  • Members
  • PipPipPip
  • 124 posts
  • Locationtexas

Posted 30 April 2012 - 03:48 PM

If you can't find and article or link, just ask Matt Oz. He can find anything! Posted Image
juli

La Paloma Texas Pottery, Juli Long


#4 Matt Oz

Matt Oz

    Advanced Member

  • Members
  • PipPipPip
  • 308 posts
  • LocationMichigan

Posted 30 April 2012 - 04:25 PM

If you can't find and article or link, just ask Matt Oz. He can find anything! Posted Image
juli


I'm still looking for the link to the meaning of life ;)

#5 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,681 posts
  • LocationNorthern Virginia

Posted 30 April 2012 - 05:11 PM


If you can't find and article or link, just ask Matt Oz. He can find anything! Posted Image
juli


I'm still looking for the link to the meaning of life ;)


Look no further . . . http://en.wikiquote.org/wiki/Monty_Python's_The_Meaning_of_Life

#6 Matt Oz

Matt Oz

    Advanced Member

  • Members
  • PipPipPip
  • 308 posts
  • LocationMichigan

Posted 30 April 2012 - 05:31 PM



If you can't find and article or link, just ask Matt Oz. He can find anything! Posted Image
juli


I'm still looking for the link to the meaning of life ;)


Look no further . . . http://en.wikiquote.org/wiki/Monty_Python's_The_Meaning_of_Life


I should have known you'd have the missing link.

#7 Ginny C

Ginny C

    Advanced Member

  • Members
  • PipPipPip
  • 118 posts
  • LocationFort Wayne, IN

Posted 30 April 2012 - 08:56 PM




If you can't find and article or link, just ask Matt Oz. He can find anything! Posted Image
juli


I'm still looking for the link to the meaning of life ;)


Look no further . . . http://en.wikiquote.org/wiki/Monty_Python's_The_Meaning_of_Life


I should have known you'd have the missing link.





#8 Ginny C

Ginny C

    Advanced Member

  • Members
  • PipPipPip
  • 118 posts
  • LocationFort Wayne, IN

Posted 30 April 2012 - 08:58 PM

Thanks, Matt. And you all brought a chuckle...glad to have given the opportunity for some levity about life in the responses!

Ginny

#9 Diana Ferreira

Diana Ferreira

    opinionated ignoramus

  • Members
  • PipPipPip
  • 186 posts
  • LocationCape Town, South Africa

Posted 01 May 2012 - 01:37 AM

Hi, when you fire your pot, place it on a slab of clay. It will shrink in the kiln with the slab, and the feet will not 'pull off' because it gets stuck on the kiln floor. I will also add some Alumina on the slab, just to be cautious.
Diana
www.dianaferreiraceramics.com
https://www.facebook...70824173&type=3

#10 SmartsyArtsy

SmartsyArtsy

    Chris Seminara

  • Members
  • PipPipPip
  • 182 posts
  • LocationPNW

Posted 01 May 2012 - 05:34 PM

Diana, I don't understand why the feet would fall off. I've fired several pots like this with no problem (^6)