Jump to content

Recommended Posts

Loaded kiln for one fire porcelain to reach 1240. At around 350 degs realized I had forgotten to put some beads that I meant to fire So opened kiln gingerly ..... Will this seriously affect the rest of my firing

Yikes !!!

Share this post


Link to post
Share on other sites

You get the beads in???

Prob not but hope the beads were very dry or they may explode....

Top or front loader?

Depends also if there was a big drop in temp.

Fingers crossed.

Share this post


Link to post
Share on other sites

If they blow expect attachments to your glazed pieces andvacuum kiln thoroughly, element and chanels esp

Let's k now how you got on.

Really worth cooling in this type of situation as Neil said , a lot at stake.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.


×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.