Kate Reeves Posted June 12 Report Share Posted June 12 (edited) Hi I made the following glaze which is fabulous and I must share!... Its a deep turquoise blue green. Potash Feldspar 1920g Dolomite 640g Quartz 480g China Clay 160g Rutile 1% 32g Cobalt Carbonate 1% 32g Chromium 1% 32g Edited June 12 by Kate Reeves Quote Link to comment Share on other sites More sharing options...
Bam2015 Posted June 12 Report Share Posted June 12 Thank you for sharing. Do you have a picture? Betty Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
Min Posted June 12 Report Share Posted June 12 @Kate Reeves, kind of you to share, would you please include the cone for the recipe in case some people don't realize this would be a high fire glaze. thanks Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
Kate Reeves Posted June 15 Author Report Share Posted June 15 Hello, sorry i'm getting used to all this technology with the pictures! (single dip (bottom) and double dip (top)) I use stoneware clay and temp 1245. thanks Kate Hulk, Kelly in AK and Rae Reich 3 Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.