dawn neusinger Posted February 6 Report Share Posted February 6 Hi. Pls advise. Bisqued clay earthenware at (pn3) 1160⁰c , can I still color glaze in second firing? Or is item no longer porous and will simply melt off in firing? Thx Quote Link to comment Share on other sites More sharing options...
Kelly in AK Posted February 6 Report Share Posted February 6 You can glaze them, it may be a challenge.Warm the pots, spray the glaze. Thin layers with, ample time to dry between coats. Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
Babs Posted February 6 Report Share Posted February 6 That's getting up there! What firing range is written on the bag? Do as Kelly suggests but I'd be tempted to do just a couple as could be unsuccessful. Won't turn out like a pot bisqued to C 06 or 04. Would be nearing the end if its firing range at C 3 and if red clay the coloyr wiuld be pretty dark. Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.