Hi. Pls advise. Bisqued clay earthenware at (pn3) 1160⁰c , can I still color glaze in second firing? Or is item no longer porous and will simply melt off in firing? Thx
Used normal candle wax on pottery, it burnt black and caused major black smoke. Switched off electric kiln and removed all burnt pottery. Shelves are now blackened and likely have trace elements of wax, how can I remove the blackened marks? And can I then empty fire shelves to remove all possible elements. Or are shelves now permanently blackened where objects burnt. Thanks dawn