Hey there! I recently bought a used Evenheat Rampmaster II 2322 kiln. It’s my first time with a computerized kiln. I did a Fast Bisque program test fire with an empty kiln to 06 and it seemed to be working well but after 3 hours it had an Error 1 code and it said the temp it turned off was around 1400. I figured it was old elements bc they look kind of worn but I tested them with a multimeter tool and the Ohms weren’t that high, only about .25 to .5 ohms higher. When I opened up the kiln though, the Cone 06 witness cone was completely melted in a blob to the shelf. If it only is reading 1400 but obviously went way past Cone 06, so you think this is a thermocouple issue? Looking at the thermocouple I don’t see a ton of wear on the tip or anything obvious. This is my first digital kiln experience and I need help. I’ve tried contacting Evenheat but haven’t heard back yet and I’m not sure what their tech support is like. Thanks for any and all diagnostic help!

Link to comment
Share on other sites

@Ariel23 I suggest changing the title of your post to better reflect the content so you get more replies.

Definitely check the program and see if you accidentally put in cone 6 instead of 06. If the controller said it only got to 1400F but it melted cone 06 to a blob, then check if the controller is set for F or C, and also check to make sure it's set to the correct type of thermocouple that you have.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.