Gonen Posted March 19, 2023 Report Share Posted March 19, 2023 hi all can i mix chromium oxide or Manganese Oxide in water to emphasize texture as i do with copper and iron oxide? should they be covered with transparent glaze? Quote Link to comment Share on other sites More sharing options...
Mark C. Posted March 19, 2023 Report Share Posted March 19, 2023 If its non -functional who cares? Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
Min Posted March 19, 2023 Report Share Posted March 19, 2023 What cone are you firing to and are the pots non functional? Chrome will be quite dry and rough without flux added at both low and midrange. Gonen 1 Quote Link to comment Share on other sites More sharing options...
neilestrick Posted March 19, 2023 Report Share Posted March 19, 2023 If you have access to them, you could also just use a commercial underglaze and get the same effect. They come in a million colors and are already fluxed out. Quote Link to comment Share on other sites More sharing options...
KB3d Posted April 4, 2023 Report Share Posted April 4, 2023 So I think you are wondering if these highly toxic glazes will be poisonous by touching them on the finished surface. I don’t know if they would be harmful like this, but to ease your mind, you could coat with a matte clear glaze to insure that they would be covered without messing with your look. Quote Link to comment Share on other sites More sharing options...