cusher Posted May 28, 2022 Author Report Share Posted May 28, 2022 Thanks all.. I will replace the elements and switch . Will keep updated. Still surprisingly expensive these parts! Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted May 29, 2022 Report Share Posted May 29, 2022 16 minutes ago, cusher said: Thanks all.. I will replace the elements and switch . Will keep updated. Still surprisingly expensive these parts! The switch is likely good - still, not a very expensive renewal though and a good idea in case it is not very calibrated after years of use.. Keep the old one as a spare if you do replace. You are confident you measured infinity on element #2 and ALL your elements measured above 10% greater resistance. You definitely need elements. Quote Link to comment Share on other sites More sharing options...
cusher Posted July 27, 2022 Author Report Share Posted July 27, 2022 So an update on this. There was one element that was broken I replaced it, I chipped out and did not buy all new elements for the rest of the levels, the Kim still would not reach cone six my concern is that because it’s so old, Even if I replace the elements it will still not reach cone six..? even if I replace the elements it will still not reach con six. Paragon is no help their customer service is terrible it’s basically one person servicing the entire world. I had to get Cole so many times to get any information. The max temp on the Kim says 2300 so therefore it should reach con six it has basically stalled out at 1600° every firing. It was wired professionally by an electrician so I don’t know what’s going on should I just make the gamble and spend the money on replacing all the elements? It’s quite expensive Quote Link to comment Share on other sites More sharing options...
cusher Posted July 27, 2022 Author Report Share Posted July 27, 2022 Also to add to this I’m testing the other elements, they all essentially test fine with my cheap on meter which is .5 resistance anyways meaning it doesn’t zero properly, Quote Link to comment Share on other sites More sharing options...
cusher Posted July 27, 2022 Author Report Share Posted July 27, 2022 On 5/28/2022 at 8:04 PM, Bill Kielb said: The switch is likely good - still, not a very expensive renewal though and a good idea in case it is not very calibrated after years of use.. Keep the old one as a spare if you do replace. You are confident you measured infinity on element #2 and ALL your elements measured above 10% greater resistance. You definitely need elements. Bill would you ever be willing to hop on a short call to discuss this further, I have found your advice very helpful. Quote Link to comment Share on other sites More sharing options...
cusher Posted July 27, 2022 Author Report Share Posted July 27, 2022 The cost of replacing all the elements is near $800, which is just really expensive to me right now Quote Link to comment Share on other sites More sharing options...
Pres Posted July 27, 2022 Report Share Posted July 27, 2022 I was away in May folks and missed this so I moved it here as it seems to be a repair issue. best, Pres Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted July 27, 2022 Report Share Posted July 27, 2022 4 hours ago, cusher said: Bill would you ever be willing to hop on a short call to discuss this further, I have found your advice very helpful. Sure DM me - envelop at the top of the screen Quote Link to comment Share on other sites More sharing options...
cusher Posted August 2, 2022 Author Report Share Posted August 2, 2022 Let me know if you got my dm bill thanks. Any other thoughts from the public? Quote Link to comment Share on other sites More sharing options...
neilestrick Posted August 2, 2022 Report Share Posted August 2, 2022 With worn elements that were still heating it would get past 1600F. Stalling that early means there are elements not getting power, or not getting full power. Have you confirmed that all elements glow on high? If they all glow then it's possibly a switch that sticking randomly. Euclids probably has elements at a much better price. Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.