GoodKarma Posted January 27, 2022 Report Share Posted January 27, 2022 Hello! May be a silly question, but... My elements are going out, (not drooping or broken, just taking 5+ extra hrs to fire to cone 6).... and I have elements on backorder, BUT they aren't going to get here for a few months, so I was wondering if I can fire a couple of loads in the meantime or if that would damage my kiln? Link to comment Share on other sites More sharing options...
Mark C. Posted January 27, 2022 Report Share Posted January 27, 2022 No it will just take longer and longer and use more juice Link to comment Share on other sites More sharing options...
neilestrick Posted January 27, 2022 Report Share Posted January 27, 2022 You also run the risk of them not being able to get to temp at some point, which could result in some work getting ruined. If you're waiting on elements from Skutt, try Euclids. I believe they have element wire in stock and can make what you need. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.