docweathers Posted August 28, 2021 Report Share Posted August 28, 2021 What is the lowest firing temperature for Bisque Fix. I tried calling Amaco. I got an answering machine to leave a message. After two weeks there has been no return call. I think they're closed. Link to comment Share on other sites More sharing options...
winstonzeddmore Posted August 29, 2021 Report Share Posted August 29, 2021 Larry, I checked on Amaco’s website and found this: “fire to the temperature of the clay and glaze that you are using -- up to Cone 10 (2381°F, 1305°C).” I assume that since a low end isn’t specified, any low end temp will work. Hope that helps. Link to comment Share on other sites More sharing options...
docweathers Posted August 29, 2021 Author Report Share Posted August 29, 2021 Thanks I found that too. I did not know what that meant for low end. I want to use it at around 1400 with some glass. Link to comment Share on other sites More sharing options...
Mark C. Posted August 29, 2021 Report Share Posted August 29, 2021 I use it at cone 10 but it works at cone 06 as well during a bisque-1,400F means just try it I just got some from Sheffield a couople days ago - free shipping Link to comment Share on other sites More sharing options...
docweathers Posted August 29, 2021 Author Report Share Posted August 29, 2021 Okay, I will give it a try. Thanks Link to comment Share on other sites More sharing options...