JF_Potter Posted June 17, 2021 Report Share Posted June 17, 2021 I have a good homemade sink trap for my clay I throw on my wheel, but since casting slip is deflocculated, it obviously won't settle out. How do others clean their equipment they use to slip cast like measuring cups, etc?? Link to comment Share on other sites More sharing options...
Mark C. Posted June 17, 2021 Report Share Posted June 17, 2021 I used to let it dry out and tap it off since its so sticky Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted June 17, 2021 Report Share Posted June 17, 2021 If you do a wet cleanup and need the bucket water to settle out, hit it hard with some saturated epsom salt solution. You won’t be able to reclaim it as casting slip though. Link to comment Share on other sites More sharing options...