dconstantin Posted March 1, 2021 Report Share Posted March 1, 2021 Hi there, Wondering if there is any way to remove the burning marks from the Kanthal wire that got into these earrings. I have been using some wire for 1 year and these marks were not present but now I used some brand new wire that ruined my pieces. See some pictures below: Thank you https://imgur.com/7a4QpXO https://imgur.com/AAfM0v2 Link to comment Share on other sites More sharing options...
Mark C. Posted March 1, 2021 Report Share Posted March 1, 2021 i could not open photos on second try they worked-looks like its in the glaze. Link to comment Share on other sites More sharing options...
Bill Kielb Posted March 1, 2021 Report Share Posted March 1, 2021 I don't think that can be easily fully removed. likely that wire began to melt and stained the glaze. Potentially China paint around and through with gold to cover comes to mind. Link to comment Share on other sites More sharing options...
neilestrick Posted March 1, 2021 Report Share Posted March 1, 2021 I agree with Bill- the staining is likely permanently in the glaze, not just a surface effect. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.