DirtRoads Posted July 13, 2020 Report Share Posted July 13, 2020 I've only seen one other piece do this and that was 6 or 7 years ago when I accidentally fired a bisque kiln on fast with no preheat and only 1 piece did it then. I had 3 pieces do this. One ornament completely flaked in half. Nothing changed and the pieces were dry. I'm not sure if this was pugged clay or not. It happened on 2 cross plates. I personally made both of these. We have used these same imprints 100's times and have not seen this. Link to comment Share on other sites More sharing options...
Mark C. Posted July 13, 2020 Report Share Posted July 13, 2020 could be lime pops? just a thought-same clay as usual Link to comment Share on other sites More sharing options...
DirtRoads Posted July 13, 2020 Author Report Share Posted July 13, 2020 Yes same clay Laguna #60. Only clay I've ever used. Strange that it's only happened to 1 piece 6 or 7 years ago and now .... 3 pieces in one bisque load. I'll research lime pops. Link to comment Share on other sites More sharing options...
oldlady Posted July 13, 2020 Report Share Posted July 13, 2020 and toss the rest of that particular "batch" of clay if possible. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.