MisterP Posted October 18, 2019 Report Share Posted October 18, 2019 Is it possible to get the 'rust breaking' effect in a cone 6 electric glaze or is that effect limited to cone 10? I'm talking a glaze or technique that where it breaks over texture leaves a trail that looks like rust. I only have access to cone 6 electric at the moment. Thanks for the info. Link to comment Share on other sites More sharing options...
dhPotter Posted October 18, 2019 Report Share Posted October 18, 2019 Look up Cream Rust cone 6 glaze. Link to comment Share on other sites More sharing options...
liambesaw Posted October 18, 2019 Report Share Posted October 18, 2019 Bucks cream breaking rust looks great, but it's got a lot of tin so it's pricey to mix Link to comment Share on other sites More sharing options...