have you ever seen a pot with large feldspar chunks wedged into the clay?

 

i love that look, but am curious where you get the large chunks. and do you throw with them in the clay, or just smack them in the pot after you finish throwing? does anyone know?

Share this post


Link to post
Share on other sites
Guest JBaymore

I crush local feldspar and granite rocks and include them in my bodies. New Hampshire is "The Granite State", after all wink.gif . I throw with them in the clay.

 

Also check out Clay Planet's "Grogzilla" clay if you want something "readymade". http://shop.clay-pla.../grogzilla.aspx

 

best,

 

......................john

Share this post


Link to post
Share on other sites

have you ever seen a pot with large feldspar chunks wedged into the clay?

 

i love that look, but am curious where you get the large chunks. and do you throw with them in the clay, or just smack them in the pot after you finish throwing? does anyone know?

 

 

Here are pics of one my bottles from my most recent anagama firing. The detail pic shows crushed feldspar melting out. The feldspar was wedged into the clay. A bit rough on the hands but worth it.

 

Jim

post-837-132925685696_thumb.jpg

post-837-132925686861_thumb.jpg

post-837-132925685696_thumb.jpg

post-837-132925686861_thumb.jpg

Share this post


Link to post
Share on other sites

Wow Off center! Great pieces and beautiful surface.

 

 

I just asked for a free sample of feldspar grit. I want to put some in a few pieces for the precenference wood firing I am attending. I live in an area where wood is picked up every mont..or else we'd be in a jungle so there is potential here.

Marcia

Share this post


Link to post
Share on other sites

Wow Off center! Great pieces and beautiful surface.

 

 

I just asked for a free sample of feldspar grit. I want to put some in a few pieces for the precenference wood firing I am attending. I live in an area where wood is picked up every mont..or else we'd be in a jungle so there is potential here.

Marcia

 

 

Thanks, Marcia.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.