Kaolinwasher Posted June 8, 2017 Report Share Posted June 8, 2017 its taken me over one year to get to my 1st pot after being out of pottery for 11 years the stone next to the porceal test is brownstone from wisconsin and is the same stone used to make the james J hill house . It was a popular stone from the 1800s i used it at 32% in the porcealinbody . along with 24 feldspar and 50% kaolin Link to comment Share on other sites More sharing options...
Fred Sweet Posted June 8, 2017 Report Share Posted June 8, 2017 Kaolinwasher- Am I missing something? The recipe you cite totals 106. Are you referring to parts vs %? Inquiring minds, you know. Regards, Fred Link to comment Share on other sites More sharing options...
oldlady Posted June 9, 2017 Report Share Posted June 9, 2017 nice pot! great color! welcome back! Link to comment Share on other sites More sharing options...
Marcia Selsor Posted June 9, 2017 Report Share Posted June 9, 2017 The speckled coloraation is very nice. Great color. and yes, welcome to the forum. Marcia Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.