wabou5 Posted May 23, 2016 Report Share Posted May 23, 2016 Hi all, I'm very new to ceramics and need help with underglaze and clear glaze compatibility. I use Duncan covercoat on bisque with a Colorobbia CLA3 non toxic clear glaze over it. The problem is, the color just doesn't come out right when I use this glaze. I have tried firing at higher temperatures, I have tried putting the covercoat on leather hard clay, firing, then dipping in clear glaze and firing again- nothing seems to work. The color doesn't come out. I have contacted both Duncan and Colorobbia, both seem to say that the two products should work just fine together. When I tried a different clear glaze (lead based) it seemed to work perfectly fine, the color comes out just right. The problem is I do not want to be using a lead based glaze as my pots are for dinnerware! Any suggestions or ideas would be greatly appreciated!Thanks!! Link to comment Share on other sites More sharing options...
High Bridge Pottery Posted May 23, 2016 Report Share Posted May 23, 2016 I have seen talk about zinc free clear glazes that are designed for some underglaze. What colour are you trying to get? Link to comment Share on other sites More sharing options...
wabou5 Posted May 23, 2016 Author Report Share Posted May 23, 2016 Hi Joel, I'm trying to get this dark blue color! Link to comment Share on other sites More sharing options...
preeta Posted May 23, 2016 Report Share Posted May 23, 2016 have you tried a different clay body? sometimes in my experience i have found clear affects colour based on claybodies. do you have access to mayco clear glazes? or even Duncan's Pure Brilliance clear glaze Link to comment Share on other sites More sharing options...
High Bridge Pottery Posted May 23, 2016 Report Share Posted May 23, 2016 'Zinc has a complicated color response. It can have harmful and helpful effects on blues, browns, greens, pinks and is not recommended with copper, iron, or chrome.' https://digitalfire.com/4sight/oxide/zno.html It also say that zinc is not really an active flux below cone02-03. The only info I could find on the glaze seemed to have it firing under 1000c, unsure if they are using zinc in the glaze but I would guess there is some in instead of lead. Link to comment Share on other sites More sharing options...
Pugaboo Posted May 23, 2016 Report Share Posted May 23, 2016 I use a lot of Underglazes and had loads of issues until I switched tossing free clear. T Link to comment Share on other sites More sharing options...
wabou5 Posted May 23, 2016 Author Report Share Posted May 23, 2016 Thanks all!I will try to change clay bodies and see if that works!Also thanks about the zinc info. The problem is that I unfotunately dont have access to Amaco or Duncan's pure brilliance. It would be very expensive for me to get as I live abroad! Only glaze available in my country is Colorobbia! Link to comment Share on other sites More sharing options...