AndreaB Posted January 22, 2016 Report Share Posted January 22, 2016 Evening all, Quick question - Can you recycle slip cast mistakes? Link to comment Share on other sites More sharing options...
BeckyH Posted January 22, 2016 Report Share Posted January 22, 2016 Yes. You need to dry the piece then break it into small bits and rehydrate by weight to the viscosity you want. Once it's throughly mixed, let it sit overnight to clear out the aeration. You will need to add flocculants to keep the slip in proper suspension when you cast with it. Link to comment Share on other sites More sharing options...
Chilly Posted January 23, 2016 Report Share Posted January 23, 2016 You can add a certain percentage without needing to add anything other than water. Can't remember right now what that % is, but you will probably find it through google. Link to comment Share on other sites More sharing options...
AndreaB Posted January 23, 2016 Author Report Share Posted January 23, 2016 Thanks. I'll do that. Have a good weekend 👠Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.